Regarding the slow cooling of wear-resistant welding wire after surfacing
Regarding the slow cooling of wear-resistant welding wire after surfacing
To prevent cracking and peeling of the deposited metal layer, slow cooling must be carried out after the deposition. The slow cooling method can use asbestos or wood ash, aluminum silicate, and other materials to cover the weld overlay metal; It can also be cooled with the heating furnace. For surfacing metals with a high tendency towards quenching, such as high chromium cast iron welding wire, tungsten carbide wear-resistant welding wire, cobalt based welding wire, etc. After welding, it should be tempered at 600-700 ℃ for 1 hour and then slowly cooled to prevent cracking. For weld deposited metals with low quenching tendency, such as 1Cr13 and 2Cr13 weld deposited valves, air cooling can be used to obtain higher hardness after welding, and no heat treatment is required after mechanical processing.
Iboke Company is a professional manufacturer and processor of welding wire and electrode products. The company mainly produces wear-resistant welding wire, wear-resistant welding rod, overlay welding rod, flux cored welding wire, tungsten carbide alloy welding rod, stainless steel welding wire, stainless steel welding rod, copper welding wire, aluminum welding wire, silver welding wire, etc. The company has a complete and scientific quality management system. The company began producing wear-resistant welding electrodes in 1992 and was the earliest enterprise in Hebei Province to produce wear-resistant welding electrodes. With nearly 20 years of production technology and experience, our products are of excellent quality and our reputation satisfies every customer.
Previous Page: